Changes in the structure of hematite by extended dry ...
The conversion of the 80% of initial hematite to amorphous phase during extended dry grinding by tumbling, planetary and vibratory mills, needs 4000, 8500 and 50,000 kJ/kg energy respectively. It was understood that vibratory mill introduces the minimum lattice strain and gives the largest crystallites when applying the same level of stress energy.